Go to homepage

BAER HSSE-PM-TiAlN Machine Tap Form B - M 24 x 3.0 - DIN 376 nickel-based superalloy


Our machine taps are powerful and reliable taps for efficient machining in one step with the machine. Machine taps are used especially in industrial manufacturing. They can be used in CNC machines, thread cutting machines, cordless drills and pneumatic tapping arms, among others. As they are characterised by high efficiency and low production costs, they are often used in series production. The thread is cut by machine in one operation. Thus, although the BAER machine tap can basically be compared to short machine tap, it is designed for use with the machine.
The screw tap has an overflow shank according to DIN 376. This means that the shank has a smaller diameter than the thread. This means that the screw tap can also be used in deeper holes and longer thread lengths. This means that the
can also be used in deeper holes and longer thread lengths, as the long chamfer, the straight flutes and the spiral point ensure that the chip is transported forwards out of the hole. Every material has its own individual chip behaviour. Therefore, screw taps must have the correct rake angle and - for even better results - a specially treated surface. This is the only way to achieve a good chip transport and to produce a thread that is true to gauge.
The high quality of the powder-metallurgical HSSE-PM steel we use ensures that our tools are extremely durable and robust. Due to special hardening processes and repeated tempering the hardness structure is very homogeneous, which forms the ideal basis for a genuine BAER screw taps. This increases the toughness and stability of the screw taps, allowing them to remain in use for longer.
The TiAlN coating is more resistant to friction and heat and therefore offers performance advantages at high temperatures, few cooling options (such as with small dimensions and deep holes) and faster cutting speeds (more than 60 m/min). TiAlN also has advantages when machining poorly machinable and wearable materials and can also be used dry to a limited extent. Recoating of TiAlN tools is possible up to 5 times without removing the old coating

Dimensions

Diameter 24
Nominal diameter in inches 0,945
Nominal diameter in mm 24
Pitch 3
Pitch in mm 3
Dimension M 24 x 3,0
Square 14,5 mm

Characteristics

Product group Screw taps
Product type Machine taps
Thread standard M: Metric ISO standard thread according to DIN 13
Tolerance ISO2/6H
Direction Right
Standard DIN 376
Tensile strength at room temperature up to 1200 N/mm² | 38 HRC
Material HSSE-PM TiAlN

Technical information – Screw taps

Schematic representation of Core hole diameter
Core hole diameter
21 mm
Schematic representation of Hole type
Hole type
Through hole up to 2.5 x D
Schematic representation of Form / Geometry
Form / Geometry
Form B with spiral point
Schematic representation of Chamfer
Chamfer
4-5 threads
Schematic representation of Chip removal
Chip removal
Chips are removed downwards in the direction of cutting
Schematic representation of Cooling
Cooling
External cooling and lubrication
Schematic representation of Material
Material
HSSE-PM TiAlN
Schematic representation of Tensile strength at room temperature
Tensile strength at room temperature
up to 1200 N/mm² | 38 HRC
Schematic representation of Tolerance: ISO2/6H
Tolerance
ISO2/6H

Applications

  • Special nickel alloys Incoloy 825, Inconel 718, Nimonic 75, Hastelloy X
  • Stainless steels, INOX, V2A, V4A
  • Difficult-to-machine materials up to a maximum of 1200 N/mm²
  • Alloyed heat-treatable steels, nodular cast iron, malleable cast iron
  • Cast aluminium and wrought alloys Si<5% (long-chipping)
  • Copper alloys and brass (long-chipping)
  • Thermosets and moulding materials

Technical drawing

Technical drawing screw tap overrun shank
D1 M 24 x 3.0
D2 18 mm
L1 160 mm
L2 36 mm
Diameter 24
Square 14,5 mm

Application – Sample materials

Nickel alloys Cutting speed vc in m/min
2.4858 NiCr21Mo (Incoloy 825) 6 - 8
2.4668 NiCr19Fe19NbMo (Inconel 718) 6 - 8
2.4630 Ni-Cr20Ti (Nimonic 75) 6 - 8
2.4665 NiCr22Fe18Mo (Hastelloy X) 6 - 8
Stainless steels (ferritic, austenitic, martensitic) Cutting speed vc in m/min
1.4104 X14CrMoS17 10 - 12
1.4301 X5CrNi18-10 (V2A) 10 - 12
1.4571 X6CrNiMoTi17-12-2 (V4A) 10 - 12
1.4005 X12CrS13 6 - 8
Alloyed steels, quenched and tempered steels Cutting speed vc in m/min
1.8515 31CrMo12 5 - 10
1.0503 C45 25 - 30
1.7218 25CrMo4 5 - 25
1.6511 36CrNiMo4 5 - 25
Spheroidal graphite cast iron, malleable cast iron Cutting speed vc in m/min
EN-JS-1030 EN-GJS-400-15 (GGG40) 20 - 25
EN-JS-1070 EN-GJS-700-2 (GGG70) 20 - 25
EN-JM-1010 EN-GJMW-350-4 (GTW-35) 20 - 25
EN-JM-1140 EN-GJMB-450-6 (GTS-45) 20 - 25
Pure aluminum, aluminum cast and wrought alloys Si < 5% (long chip length) Cutting speed vc in m/min
Al99.5 EN AW-1050 30 - 40
AlMgSi EN AW-6060 30 - 40
AlZn5Mg3Cu EN AW-7022 30 - 40
AlMg5 EN AC-51300 15 - 18
Copper alloys, brass (long-chipping) Cutting speed vc in m/min
E-Cu 57 EN CW400A 15 - 18
CuZn37 EN CW 508 L (Ms58) 15 - 18

Cutting speed vc [m/min] = (Outer diameter * π * speed) / 1000

Rotation speed n [1/min] = (Cutting speed in m/min * 1000) / (Outer diameter * π)

Feedrate programming [mm/min] = speed * pitch

Please note that the above cutting speeds are indicative and must be adjusted depending on lubrication and actuation.

0 of 0 reviews

Average rating of 0 out of 5 stars

Leave a review!

Share your experiences with other customers.


Zubehör

BAER High Performance Cutting Paste 100 ml Express in Germany
BAER High Performance Cutting Paste 100 ml
(294)
  • Order within 10 h 8 min, estimated delivery Fri 20 Nov – Mon 23 Nov
  • Express shipping within Germany: order by 13:00, delivery tomorrow
In stock Item no. SP100
€10.72 Prices incl. VAT
HSS Drill Bit (reduced shank 13mm) 21.00 mm Express in Germany
HSS Drill Bit (reduced shank 13mm) 21.00 mm
(42)
  • Order within 10 h 8 min, estimated delivery Fri 20 Nov – Mon 23 Nov
  • Express shipping within Germany: order by 13:00, delivery tomorrow
In stock Item no. 10210043
€28.74 Prices incl. VAT
BAER Round Cutting Die M 24 x 3.0 - HSSE for Stainless Steel Express in Germany
BAER Round Cutting Die M 24 x 3.0 - HSSE for Stainless Steel
(23)
  • Order within 10 h 8 min, estimated delivery Fri 20 Nov – Mon 23 Nov
  • Express shipping within Germany: order by 13:00, delivery tomorrow
In stock Item no. 111405022
€130.15 Prices incl. VAT
Thread Plug Gauge M 24 x 3.0 - tolerance 6H
Thread Plug Gauge M 24 x 3.0 - tolerance 6H
In stock Item no. 112101011
€118.37 Prices incl. VAT
BAER High Performance Cutting Paste 500 ml Express in Germany
BAER High Performance Cutting Paste 500 ml
(27)
  • Order within 10 h 8 min, estimated delivery Fri 20 Nov – Mon 23 Nov
  • Express shipping within Germany: order by 13:00, delivery tomorrow
In stock Item no. SP5000
€30.32 Prices incl. VAT

Subscribe to our newsletter

To receive the latest information and be the first to know about new products, leave us your e-mail address.

Please accept the privacy policy to subscribe to the email newsletter.